92国产精品午夜福利免_18欧美乱大交欧美日韩a_在线观看国产精品乱码app_十八禁 又黄又大视频网站_日韩加勒比一本无码精品群玩_在线观看国产成人aⅤ天堂_av大片免费播放网站_国产精品开放后亚洲_日韩AV在第一页_男女裸交啪啪激高潮出水

中文版 | English

Common problemLocation: Home > service support >Common problem

Position offset of bottom nozzle of PET bottle

Reasons: 1, start blowing time early 2, stretching rod didn't exactly 3, stretching rod and bottle of shaft centerline offset 4, germ tube wall thickness uneven or injection of uneven density 5, heating uneven

 

Exclusion method: 1, delay blowing time or increasing tensile bar decreased 2, speed adjusting magnetic pole switch position 3, adjust the stretching rod position 4, improve the embryo quality 5, improving the heating conditions, or embryo test tube autorotation has